Glossary » Materials » Polymers » Polysulfone » 20% Glass Fiber Reinforced
20% Glass Fiber Reinforced PSU is a subcategory of Polysulfone. The additative is added by weight during the manufacturing process.
Polysulfone, also known as PSU, is a thermoplastic polycondensate. The most common trade name is Ultrason. polysulfone It is an expensive material. It is electroplatable and has high strength, good toughness, good dielectric strength, and dimensional stability. It is commonly used in electric connectors.
Additional Information
Other common Polysulfone (PSU) include Injection Molding, Flame-Retardant, Extrusion PSU, Mineral Filled PSU, Extrusion / Injection Molding Grade PSU, 30% Carbon Fiber EMI Shielding (conductive) PSU, Injection Molding, Platable Grade PSU, PSU, Unfilled PSU, 10% Glass Fiber Reinforced PSU, 20% Glass Fiber Reinforced PSU, 30% Carbon Fiber EMI Shielding (conductive) PSU, PSU, Unreinforced PSU, and Mineral Filled PSU.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 418
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Alloys: Steel: Tool Steel
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A517 Grade P
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 5454
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Polymers: Cellulosic: Ethyl Cellulose: Molding Compound and Sheet
Glossary: Materials: Polymers: Polyphenylene Sulfide: 30% Glass Fiber Reinforced
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Alloys: Steel: Tool Steel
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A517 Grade P
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 5454
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Polymers: Cellulosic: Ethyl Cellulose: Molding Compound and Sheet
Glossary: Materials: Polymers: Polyphenylene Sulfide: 30% Glass Fiber Reinforced
Related Pages
eFunda Polymers: Properties of Sulfone polymers {polysulfone ...
eFunda Polymers: Properties of Sulfone polymers {polysulfone, injection molding, platable grade}
eFunda Polymers: Properties of ABS {20% long glass fiber ...
eFunda Polymers: Properties of ABS {20% long glass fiber reinforced, injection molding grade} ... Additives: 20% long glass fiber reinforced ...
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111 ... Bamberger Polymers, Inc. 2 Jericho Plaza. Jericho, NY 11753 ...
eFunda Polymers: Listing of Polysulfone (Ultrason)
Polysulfone, also known as PSU, has been mass-produced since 1965. ... Sulfone polymers, polysulfone, 30% carbon fiber, EMI shielding (conductive). ...
eFunda: Polymer (Plastic) Supplier Contact Information
American Polymers, Inc. 53 Millbrook St. P.O. Box 60398. Worcester, MA 01606 ... Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219 ...
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass ...
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass fiber reinforced} ... Additives: 20 - 30% long glass fiber reinforced ...
eFunda: Glossary of Polymers (Plastics)
Common terms used in material science of polymers.
eFunda Polymers: Listing of Liquid Crystal Polymer (Vectra, Xydar)
Liquid Crystal Polymer, also known as LCP, has been mass-produced since 1980. ... Liquid Crystal Polymer, glass fiber reinforced, used for SMT. ...
eFunda Polymers: Properties of Sulfone polymers {polysulfone, 30 ...
eFunda Polymers: Properties of Sulfone polymers {polysulfone, 30% carbon fiber, EMI shielding (conductive)}
eFunda Polymers: Properties of Sulfone polymers {modified ...
eFunda Polymers: Properties of Sulfone polymers {modified polysulfone, mineral filled} ... State: modified polysulfone. Additives: mineral filled ...