Injection Molding PVDC is a subcategory of Polyvinylidene Chloride. It is specially formulated to injection molding. Its elastic modulus ranges from 55 to 95 MPa. Its flexural modulus ranges from 55 to 95 MPa. Its tensile strength ranges from 3500 to 5000 MPa at break. Its flexural strength ranges from 4200 to 6200 MPa. Its compressive strength ranges from 2000 to 2700 MPa. Its Izod Impact strength ranges from 0.4 to 1 J/cm. Its elongation at break ranges from 160 to 240 %. Its hardness ranges from 60 to 65 Rockwell M. Its specific gravity ranges from 1.65 to 1.72. Its molding pressure ranges from 5 to 30 MPa.
Polyvinylidene Chloride, also known as PVDC, is a thermoplastic polymer. Common trade names include Diofan, Ixan, and Saran. copolymer It has high hardness and good abrasion resistance. It is typically used as one of the components in a copolymer.
Additional Information
Other common Polyvinylidene Chloride (PVDC) include Unplasticized Barrier Film Resins PVDC, and Plasticized Barrier Film Resins PVDC.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4028
Glossary: Materials: Alloys: Steel: Tool Steel: AISI A3
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C99600
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Alloys: Copper Alloy: Wire
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Alloys: Steel: Tool Steel: AISI A3
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C99600
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Alloys: Copper Alloy: Wire
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Alloys: Steel: Stainless Steel
Related Pages
eFunda Polymers: Properties of Polyvinylidene Chloride {copolymer ...
eFunda Polymers: Properties of Polyvinylidene Chloride {copolymer, unplasticized, barrier film resins}
eFunda Polymers: Properties of ABS {injection molding grade, heat ...
eFunda Polymers: Properties of ABS {injection molding grade, heat resistant}
eFunda Polymers: Properties of ABS {transparent, injection molding ...
eFunda Polymers: Properties of ABS {transparent, injection molding grade}
eFunda Polymers: Properties of ABS {30% glass fiber reinforced ...
Processing Temperature (ºC), 205 - 238, injection molding. Linear Mold Shrinkage (cm/cm), 0.002 - 0.003, D955. Top of Page. Suppliers ...
eFunda: Polymers (Plastics) Sorted by Resin Family
Polymethylpentene, (PMP). •, Polypropylene, (PP). •, Polystyrene, (PS). •, Polyvinylchloride, (PVC). •, Polyvinylidene Chloride, (PVDC). ...
eFunda Polymers: Properties of ABS {injection molding grade, platable}
eFunda Polymers: Properties of ABS {injection molding grade, platable}
eFunda: Polymer (Plastic) Supplier Contact Information
Polyvinylidene Chloride, copolymer, unplasticized, barrier film resins. Dow Plastics. 690 Bldg. Midland, MI 48640. Toll Free: 800-441-4369 ...
eFunda: Listing of Common Polymers (Plastics)
Polyvinylchloride, (PVC), Thermoplastic polymer. Polyvinylidene Chloride, (PVDC), Thermoplastic polymer. Silicone, (SI), Thermoset polycondensate. ...
eFunda Polymers: Properties of ABS {20% glass fiber reinforced ...
Processing Temperature (ºC), 177 - 260, injection molding. 177 - 260, compression molding. Molding Pressure (MPa), 104 - 207. Linear Mold Shrinkage (cm/cm) ...