Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Resources
Bibliography
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free publications
 
AISI 4023
Category Steel
Class Alloy steel
Type Standard
Common Names Molybdenum steel
Designations  United States: ASTM A322 , ASTM A331 , ASTM A519 , ASTM A534 , SAE J404 , SAE J412 , SAE J770 , UNS G40230

Composition

ElementWeight %
C  0.20-0.25 
Mn  0.70-0.90 
P  0.035 (max) 
S  0.04 (max) 
Si  0.15-0.30 
Mo  0.20-0.30 

Mechanical Properties

Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  
Glossary
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.