Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Resources
Bibliography
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

more free publications
 
AISI 4024
Category Steel
Class Alloy steel
Type Standard
Common Names Molybdenum steel
Designations  United States: ASTM A322 , ASTM A331 , ASTM A519 , SAE J404 , SAE J412 , SAE J770 , UNS G40240

Composition

ElementWeight %
C  0.20-0.25 
Mn  0.70-0.90 
P  0.035 (max) 
S  0.035-0.050 (max) 
Si  0.15-0.30 
Mo  0.20-0.30 

Mechanical Properties

Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  
Glossary
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.