| AISI 4047 | |
![]() | |
| Category | Steel |
| Class | Alloy steel |
| Type | Standard |
| Common Names | Molybdenum steel |
| Designations | United States: ASTM A322 , ASTM A331 , ASTM A519 , SAE J404 , SAE J412 , SAE J770 , UNS G40470 |
| Composition | |
![]() | |
| Mechanical Properties | |
![]() | |
| AISI 4047 | |
![]() | |
| Category | Steel |
| Class | Alloy steel |
| Type | Standard |
| Common Names | Molybdenum steel |
| Designations | United States: ASTM A322 , ASTM A331 , ASTM A519 , SAE J404 , SAE J412 , SAE J770 , UNS G40470 |
| Composition | |
![]() | |
| Mechanical Properties | |
![]() | |