| AISI 4615 | |
![]() | |
| Category | Steel |
| Class | Alloy steel |
| Type | Standard |
| Common Names | Nickel-molybdenum steel |
| Designations | United States: AMS 6290 , AMS 6290C , ASTM A322 , ASTM A331 , ASTM A505 , MIL SPEC MIL-S-7493 (A4615) , SAE J404 , SAE J412 , SAE J770 , UNS G46150 |
| Composition | |
![]() | |
| Element | Weight % |
| C | 0.13-0.18 |
| Mn | 0.45-0.65 |
| P | 0.035 (max) |
| S | 0.04 (max) |
| Si | 0.15-0.30 |
| Ni | 1.65-2.00 |
| Mo | 0.20-0.30 |
| Mechanical Properties | |
![]() | |
| Properties | Conditions | ||
| T (°C) | Treatment | ||
| Density (×1000 kg/m3) | 7.7-8.03 | 25 | |
| Poisson's Ratio | 0.27-0.30 | 25 | |
| Elastic Modulus (GPa) | 190-210 | 25 | |
| Thermal Properties | |
![]() | |