Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Resources
Bibliography
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

more free publications
 
AISI 5120H
Category Steel
Class Alloy steel
Type H-steel
Common Names Chromium steel
Designations  France: AFNOR 20 MC 5
Germany: DIN 1.7147
United States: ASTM A304 , SAE J1268 , UNS H51200

Composition

ElementWeight %
C  0.17-0.23 
Mn  0.60-1.00 
Cr  0.60-1.00 
P  0.035 
S  0.040 
Si  0.15-0.30 

Mechanical Properties

Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  
Glossary
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.