Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Further Details
Resources
Bibliography
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

more free publications
 
AISI 5140H
ConditionsElectrical Resistivity (10-9W-m)
T (°C)Treatment
20   228 
100   281 
200   352 
400   530 
600   785 
Glossary
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!