Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Resources
Bibliography
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

more free publications
 
AISI 6150H
Category Steel
Class Alloy steel
Type H-steel
Common Names Chromium-vanadium steel
Designations  France: AFNOR 50 CV 4
Germany: DIN 1.8159
Italy: UNI  5O CrV 4
Japan: JIS SUP 10
Sweden: SS 2230
United Kingdom: B.S. 735 A 50 , B.S. En. 47
United States: ASTM A304 , SAE J1268 , UNS H61500

Composition

ElementWeight %
C  0.47-0.54 
Mn  0.60-1.00 
Cr  0.75-1.20 
P  0.035 
S  0.040 
Si  0.15-0.30 
V  0.15 (min) 

Mechanical Properties

Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  

Thermal Properties

Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 14.4  20-600 more annealed more
Glossary
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.