Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Resources
Bibliography
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

more free publications
 
AISI 6150H
Category Steel
Class Alloy steel
Type H-steel
Common Names Chromium-vanadium steel
Designations  France: AFNOR 50 CV 4
Germany: DIN 1.8159
Italy: UNI  5O CrV 4
Japan: JIS SUP 10
Sweden: SS 2230
United Kingdom: B.S. 735 A 50 , B.S. En. 47
United States: ASTM A304 , SAE J1268 , UNS H61500

Composition

ElementWeight %
C  0.47-0.54 
Mn  0.60-1.00 
Cr  0.75-1.20 
P  0.035 
S  0.040 
Si  0.15-0.30 
V  0.15 (min) 

Mechanical Properties

Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  

Thermal Properties

Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 14.4  20-600 more annealed more
Glossary
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.