Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Further Details
Resources
Bibliography
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

more free publications
 
AISI 8630H
ConditionsHardness
T (°C)TreatmentMethodValue
25 annealed at 845°C   HB 156 
25 normalized at 870°C   HB 187 
Glossary
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.