AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Resources
Bibliography
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

more free publications
 
AISI 8650
Category Steel
Class Alloy steel
Type Standard
Common Names Nickel-chromium-molybdenum steel
Designations  United States: ASTM A322 , ASTM A505 , ASTM A519 , SAE J404 , SAE J412 , SAE J770 , UNS G86500

Composition

ElementWeight %
C  0.48-0.53 
Mn  0.75-1.00 
P  0.035 (max) 
S  0.04 (max) 
Si  0.15-0.30 
Cr  0.40-0.60 
Ni  0.40-0.70 
Mo  0.15-0.25 

Mechanical Properties

Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  
Tensile Strength (Mpa) 715.7  25  annealed at 795°C  more
Yield Strength (Mpa) 386.1 
Elongation (%) 22.5 
Reduction in Area (%) 46.4 
Hardness (HB) 212  25  annealed at 795°C more
Impact Strength (J)
(Izod)
29.4  25  annealed at 795°C  more
Glossary
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.