Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Further Details
Resources
Bibliography
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

more free publications
 
AISI 8650
ConditionsImpact Energy (J)
T (°C)TreatmentMethodValue
25 annealed at 795°C   Izod 29.4 
25 normalized at 870°C   Izod 13.6 
Glossary
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.