Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Resources
Bibliography
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

more free publications
 
AISI 8660
Category Steel
Class Alloy steel
Type Standard
Common Names Nickel-chromium-molybdenum steel
Designations  United States: ASTM A322 , ASTM A332 , ASTM A506 , ASTM A519 , ASTM A711 , SAE J404 , SAE J412 , SAE J770 , UNS G86600

Composition

ElementWeight %
C  0.56-0.64 
Mn  0.75-1.00 
P  0.035 (max) 
S  0.04 (max) 
Si  0.15-0.30 
Cr  0.40-0.60 
Ni  0.40-0.70 
Mo  0.15-0.25 

Mechanical Properties

Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  
Tensile Strength (Mpa) 1634  25  oil quenched, fine grained, tempered at 425°C  more
Yield Strength (Mpa) 1551 
Elongation (%) 13 
Reduction in Area (%) 37 
Hardness (HB) 580  25  oil quenched, fine grained, tempered at 205°C more
Glossary
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.