Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Resources
Bibliography
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

more free publications
 
AISI 8740H
Category Steel
Class Alloy steel
Type H-steel
Common Names Nickel-chromium-molybdenum steel
Designations  Germany: DIN 1.6546
Italy: UNI 40 NiCrMo 2 KB
United Kingdom: B.S. Type 7
United States: ASTM A304 , SAE J1268 , UNS H87400

Composition

ElementWeight %
C  0.37-0.44 
Mn  0.70-1.05 
Cr  0.35-0.65 
Ni  0.35-0.75 
Mo  0.20-0.30 
P  0.035 
S  0.040 
Si  0.15-0.30 

Mechanical Properties

Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  
Tensile Strength (Mpa) 695  25  annealed at 815°C  more
Yield Strength (Mpa) 415 
Elongation (%) 22.2 
Reduction in Area (%) 46 
Hardness (HB) 201  25  annealed at 815°C more
Glossary
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.