| SAE 980X | |
![]() | |
| Conditions | Tensile Properties | ||
| T (°C) | Treatment | ||
| 25 | (sheet and strip) | Tensile Strength (MPa) | 655 |
| Yield Strength (MPa) | 550 | ||
| Elongation (%) | 12 | ||
| Reduction in Area (%) | |||
| 25 | (sheet and strip, plate, shapes and bar to 10 mm) | Tensile Strength (MPa) | 655 |
| Yield Strength (MPa) | 550 | ||
| Elongation (%) | |||
| Reduction in Area (%) | |||