Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Further Details
Resources
Bibliography
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

more free publications
 
AA 2014
Conditions Tensile Properties 
T (°C)Treatment
25 O   Tensile Strength (MPa) 185 
Yield Strength (MPa) 97 
Elongation (%)  
Reduction in Area (%)  
25 O (Alclad)  Tensile Strength (MPa) 170 
Yield Strength (MPa) 69 
Elongation (%) 21 
Reduction in Area (%)  
25 T3 (Alclad)  Tensile Strength (MPa) 435 
Yield Strength (MPa) 275 
Elongation (%) 20 
Reduction in Area (%)  
25 T4 (Alclad)  Tensile Strength (MPa) 420 
Yield Strength (MPa) 255 
Elongation (%) 22 
Reduction in Area (%)  
25 T4   Tensile Strength (MPa) 425 
Yield Strength (MPa) 290 
Elongation (%)  
Reduction in Area (%)  
25 T6   Tensile Strength (MPa) 485 
Yield Strength (MPa) 415 
Elongation (%)  
Reduction in Area (%)  
25 T6 (Alclad)  Tensile Strength (MPa) 470 
Yield Strength (MPa) 415 
Elongation (%) 10 
Reduction in Area (%)  
Glossary
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.