Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Resources
Bibliography
STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

more free publications
 
AA 2036
Category Aluminum Alloy
Class Wrought

Composition
ElementWeight %
Al  96.70 
Cu  2.6 
Mn  0.25 
Mg  0.45 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 2.6-2.8 25  
Poisson's Ratio 0.33 25  
Elastic Modulus (GPa) 70-80 25  
Tensile Strength (Mpa) 340  25  T4  
Yield Strength (Mpa) 195 
Elongation (%) 24 
Reduction in Area (%)  
Fatigue Strength (MPa) 125  25  T4  

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Conductivity (W/m-K) 198  25  O more

Electric Properties
Properties Conditions 
T (°C)Treatment
Electric Resistivity (10-9W-m) 33  25  O more
Glossary
STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!