Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Further Details
Resources
Bibliography
Laser Focus World

Semiconductors, medical equipment, lasers, optics and aviation and aerospace.

Power Transmission

Gear drives, bearings, motors, clutches, couplings, machine controls, sensors and components.

Design-2-Part

How OEM's can make their parts better, faster, and more efficient.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

more free magazines
 
AA 2218
Conditions Tensile Properties 
T (°C)Treatment
25 T61   Tensile Strength (MPa) 405 
Yield Strength (MPa) 305 
Elongation (%)  
Reduction in Area (%)  
25 T71   Tensile Strength (MPa) 345 
Yield Strength (MPa) 275 
Elongation (%)  
Reduction in Area (%)  
25 T72   Tensile Strength (MPa) 330 
Yield Strength (MPa) 255 
Elongation (%)  
Reduction in Area (%)  