Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Further Details
Resources
Bibliography
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

more free magazines
 
295.0
Conditions Tensile Properties 
T (°C)Treatment
25 T4 (sand casting)  Tensile Strength (MPa) 220 
Yield Strength (MPa) 110 
Elongation (%) 8.5 
Reduction in Area (%)  
25 T6 (sand casting)  Tensile Strength (MPa) 250 
Yield Strength (MPa) 165 
Elongation (%) 5.0 
Reduction in Area (%)  
25 T62 (sand casting)  Tensile Strength (MPa) 285 
Yield Strength (MPa) 220 
Elongation (%) 2.0 
Reduction in Area (%)  