Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Further Details
Resources
Bibliography
STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

more free publications
 
AA 3003
ConditionsHardness
T (°C)TreatmentMethodValue
25 H12   HB500 35 
25 H14   HB500 40 
25 H16   HB500 47 
25 H18   HB500 55 
25 O   HB500 28 
Glossary
STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.