Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Further Details
Resources
Bibliography
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

more free publications
 
AA 3003
Conditions Tensile Properties 
T (°C)Treatment
25 H12   Tensile Strength (MPa) 130 
Yield Strength (MPa) 125 
Elongation (%) 10 
Reduction in Area (%)  
25 H14   Tensile Strength (MPa) 150 
Yield Strength (MPa) 145 
Elongation (%)
Reduction in Area (%)  
25 H16   Tensile Strength (MPa) 180 
Yield Strength (MPa) 170 
Elongation (%)
Reduction in Area (%)  
25 H18   Tensile Strength (MPa) 200 
Yield Strength (MPa) 185 
Elongation (%)
Reduction in Area (%)  
25 O   Tensile Strength (MPa) 110 
Yield Strength (MPa) 42 
Elongation (%) 30 
Reduction in Area (%)  
Glossary
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.