Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Further Details
Resources
Bibliography
Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

more free publications
 
AA 4043
Conditions Tensile Properties 
T (°C)Treatment
25 H18   Tensile Strength (MPa) 285 
Yield Strength (MPa) 270 
Elongation (%) 0.5 
Reduction in Area (%)  
25 O   Tensile Strength (MPa) 145 
Yield Strength (MPa) 69 
Elongation (%) 22 
Reduction in Area (%)  
Glossary
Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.