Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Further Details
Resources
Bibliography
Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

more free publications
 
AA 5005
ConditionsHardness
T (°C)TreatmentMethodValue
25 H32   HB500 36 
25 H34   HB500 41 
25 H36   HB500 46 
25 H38   HB500 51 
25 O   HB500 28 
Glossary
Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.