Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Further Details
Resources
Bibliography
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free publications
 
AA 5052
ConditionsFatigue Strength (MPa)
T (°C)Treatment
25 H32   115 
25 H34   125 
25 H36   130 
25 H38   140 
25 O   110 
Glossary
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.