Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Resources
Bibliography
Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

more free publications
 
AA 5056
Category Aluminum Alloy
Class Wrought

Composition
ElementWeight %
Al  95.0 
Mn  0.12 
Mg  5.0 
Cr  0.12 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 2.64 25  
Poisson's Ratio 0.33 25  
Elastic Modulus (GPa) 70-80 25  
Tensile Strength (Mpa) 435  25  H18  more
Yield Strength (Mpa) 405 
Elongation (%)  
Reduction in Area (%)  
Hardness (HB500) 105  25  H18 more
Shear Strength (MPa) 235  25  H18  more
Fatigue Strength (MPa) 150  25  H18  more

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 24.1  20-100  
Thermal Conductivity (W/m-K) 112  25  H38 more

Electric Properties
Properties Conditions 
T (°C)Treatment
Electric Resistivity (10-9W-m) 64  25  H38 more
Glossary
Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.