Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Further Details
Resources
Bibliography
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

more free publications
 
AA 5056
ConditionsHardness
T (°C)TreatmentMethodValue
25 H18   HB500 105 
25 H38   HB500 100 
25 O   HB500 65 
Glossary
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.