| AA 5056 | |
![]() | |
| Conditions | Tensile Properties | ||
| T (°C) | Treatment | ||
| 25 | H18 | Tensile Strength (MPa) | 435 |
| Yield Strength (MPa) | 405 | ||
| Elongation (%) | |||
| Reduction in Area (%) | |||
| 25 | H38 | Tensile Strength (MPa) | 415 |
| Yield Strength (MPa) | 345 | ||
| Elongation (%) | |||
| Reduction in Area (%) | |||
| 25 | O | Tensile Strength (MPa) | 290 |
| Yield Strength (MPa) | 150 | ||
| Elongation (%) | |||
| Reduction in Area (%) | |||