Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Further Details
Resources
Bibliography
Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

more free publications
 
AA 5083
Conditions Tensile Properties 
T (°C)Treatment
25 H112   Tensile Strength (MPa) 305 
Yield Strength (MPa) 195 
Elongation (%)  
Reduction in Area (%)  
25 H113   Tensile Strength (MPa) 315 
Yield Strength (MPa) 230 
Elongation (%)  
Reduction in Area (%)  
25 H32   Tensile Strength (MPa) 325 
Yield Strength (MPa) 250 
Elongation (%)  
Reduction in Area (%)  
25 H321   Tensile Strength (MPa) 315 
Yield Strength (MPa) 230 
Elongation (%)  
Reduction in Area (%)  
25 H323   Tensile Strength (MPa) 325 
Yield Strength (MPa) 250 
Elongation (%)  
Reduction in Area (%)  
25 H34   Tensile Strength (MPa) 345 
Yield Strength (MPa) 285 
Elongation (%)  
Reduction in Area (%)  
25 H343   Tensile Strength (MPa) 345 
Yield Strength (MPa) 285 
Elongation (%)  
Reduction in Area (%)  
25 O   Tensile Strength (MPa) 290 
Yield Strength (MPa) 145 
Elongation (%)  
Reduction in Area (%)  
Glossary
Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.