Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Further Details
Resources
Bibliography
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Machine Design

How-to, in-depth technical articles for machine design engineers

Power Transmission

Gear drives, bearings, motors, clutches, couplings, machine controls, sensors and components.

more free magazines
 
AA 5086
Conditions Tensile Properties 
T (°C)Treatment
25 H112   Tensile Strength (MPa) 270 
Yield Strength (MPa) 130 
Elongation (%) 14 
Reduction in Area (%)  
25 H116   Tensile Strength (MPa) 290 
Yield Strength (MPa) 205 
Elongation (%) 12 
Reduction in Area (%)  
25 H117   Tensile Strength (MPa) 290 
Yield Strength (MPa) 205 
Elongation (%) 12 
Reduction in Area (%)  
25 H32   Tensile Strength (MPa) 290 
Yield Strength (MPa) 205 
Elongation (%) 12 
Reduction in Area (%)  
25 H34   Tensile Strength (MPa) 325 
Yield Strength (MPa) 255 
Elongation (%) 10 
Reduction in Area (%)  
25 O   Tensile Strength (MPa) 260 
Yield Strength (MPa) 115 
Elongation (%) 22 
Reduction in Area (%)  