Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Further Details
Resources
Bibliography
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

more free publications
 
AA 5154
ConditionsHardness
T (°C)TreatmentMethodValue
25 H112   HB500 63 
25 H32   HB500 67 
25 H34   HB500 73 
25 H36   HB500 78 
25 H38   HB500 80 
25 O   HB500 58 
Glossary
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.