Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Further Details
Resources
Bibliography
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

more free publications
 
AA 5456
Conditions Tensile Properties 
T (°C)Treatment
25 H111   Tensile Strength (MPa) 325 
Yield Strength (MPa) 230 
Elongation (%)  
Reduction in Area (%)  
25 H112   Tensile Strength (MPa) 310 
Yield Strength (MPa) 165 
Elongation (%)  
Reduction in Area (%)  
25 H116   Tensile Strength (MPa) 350 
Yield Strength (MPa) 255 
Elongation (%)  
Reduction in Area (%)  
25 H321   Tensile Strength (MPa) 350 
Yield Strength (MPa) 255 
Elongation (%)  
Reduction in Area (%)  
25 O   Tensile Strength (MPa) 310 
Yield Strength (MPa) 160 
Elongation (%)  
Reduction in Area (%)  
Glossary
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.