AA 5652 | |
![]() | |


Conditions | Tensile Properties | ||
T (°C) | Treatment | ||
25 | H32 | Tensile Strength (MPa) | 230 |
Yield Strength (MPa) | 195 | ||
Elongation (%) | 12 | ||
Reduction in Area (%) | |||
25 | H34 | Tensile Strength (MPa) | 260 |
Yield Strength (MPa) | 215 | ||
Elongation (%) | 10 | ||
Reduction in Area (%) | |||
25 | H36 | Tensile Strength (MPa) | 275 |
Yield Strength (MPa) | 240 | ||
Elongation (%) | 8 | ||
Reduction in Area (%) | |||
25 | H38 | Tensile Strength (MPa) | 290 |
Yield Strength (MPa) | 255 | ||
Elongation (%) | 7 | ||
Reduction in Area (%) | |||
25 | O | Tensile Strength (MPa) | 195 |
Yield Strength (MPa) | 90 | ||
Elongation (%) | 25 | ||
Reduction in Area (%) |