Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Resources
Bibliography
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

more free publications
 
AA 7072
Category Aluminum Alloy
Class Wrought

Composition
ElementWeight %
Al  99.0 
Zn  1.0 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 2.6-2.8 25  
Poisson's Ratio 0.33 25  
Elastic Modulus (GPa) 70-80 25  
Hardness (HB500) 28  25  H12 more
Shear Strength (MPa) 62  25  H12  more

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Conductivity (W/m-K) 227  25 

Electric Properties
Properties Conditions 
T (°C)Treatment
Electric Resistivity (10-9W-m) 29  25 
Glossary
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!