Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Further Details
Resources
Bibliography
Hydraulics & Pneumatics

For design and manufacturing engineers involved in buying or specifying fluid power components and systems.

Reinforced Plastics

Informed and impartial coverage on the global composites industry.

Quality Magazine

Techniques to improve quality on the shop floor and in manufacturing planning.

NASA Tech Briefs

Innovations developed by NASA and its industry partners in a wide array of fields.

more free magazines
 
713.0
Conditions Tensile Properties 
T (°C)Treatment
25 T5 (permanent mold casting)  Tensile Strength (MPa) 220 
Yield Strength (MPa) 150 
Elongation (%) 4.0 
Reduction in Area (%)  
25 T5 (sand casting)  Tensile Strength (MPa) 210 
Yield Strength (MPa) 150 
Elongation (%) 3.0 
Reduction in Area (%)  