Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Further Details
Resources
Bibliography
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free publications
 
AISI Type 305
Conditions Tensile Properties 
T (°C)Treatment
25 annealed (plate, sheet, strip)  Tensile Strength (MPa) 480 
Yield Strength (MPa) 170 
Elongation (%) 40 
Reduction in Area (%)  
25 annealed (wire)  Tensile Strength (MPa) 515 
Yield Strength (MPa) 205 
Elongation (%)  
Reduction in Area (%)  
25 cold finished (wire)  Tensile Strength (MPa) 620 
Yield Strength (MPa) 310 
Elongation (%)  
Reduction in Area (%)  
25 cold finished and annealed (bar (up to 13 mm in diameter))  Tensile Strength (MPa) 260 
Yield Strength (MPa) 310 
Elongation (%) 30 
Reduction in Area (%) 40 
25 cold finished and annealed (bar (over 13 mm in diameter))  Tensile Strength (MPa) 515 
Yield Strength (MPa) 205 
Elongation (%) 30 
Reduction in Area (%) 40 
25 high tensile (bar, wire)  Tensile Strength (MPa) 1690 
Yield Strength (MPa)  
Elongation (%)  
Reduction in Area (%)  
25 hot finished and annealed (bar)  Tensile Strength (MPa) 515 
Yield Strength (MPa) 205 
Elongation (%) 40 
Reduction in Area (%) 50 
Glossary
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.