Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Resources
Bibliography
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

more free publications
 
AISI 1006
Category Steel
Class Carbon steel
Type Standard
Designations  United States: AMS 5041 , ASME 5041 , ASTM A29 , ASTM A510 , ASTM A545 , FED QQ-W-461 , MIL SPEC MIL-S-11310 (CS1006) , SAE J403 , SAE J412 (1005) , SAE J414 , UNS G10060

Composition
ElementWeight %
C  0.08 (max) 
Mn  0.25-0.40 
P  0.04 (max) 
S  0.05 (max) 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.872 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  
Tensile Strength (Mpa) 330  25  cold drawn (round bar (19-32 mm)) more
Yield Strength (Mpa) 285 
Elongation (%) 20 
Reduction in Area (%) 45 
Hardness (HB) 95  25  cold drawn (round bar (19-32 mm)) more

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 12.6  0-100 more  
Specific Heat (J/kg-K) 481  50-100 more  
Glossary
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!