Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Further Details
Resources
Bibliography
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Desktop Engineering

Design, simulation, test, prototyping and high performance computing.

Autonomous Vehicle Engineering

The No. 1 media source for those developing the next generation mobility solutions.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

more free magazines
 
AISI 1008
ConditionsThermal Expansion Coeff. (10-6/ºC)
T (°C)Treatment
0-100 annealed  12.6 
0-200 annealed  13.1 
0-300 annealed  13.5 
0-400 annealed  13.8 
0-500 annealed  14.2 
0-600 annealed  14.6 
0-700 annealed  15 
20-800 annealed  14.7 
20-1000 annealed  13.8 