Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Further Details
Resources
Bibliography
Desktop Engineering

Design, simulation, test, prototyping and high performance computing.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

more free magazines
 
AISI 1008
ConditionsElectrical Resistivity (10-9W-m)
T (°C)Treatment
20   130 
100   178 
200   252 
400   448 
600   725 
700   898 
800   1073 
900   1124 
1000   1160 
1100   1189 
1200   1216 
1300   1241 