Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Further Details
Resources
Bibliography
Autonomous Vehicle Engineering

The No. 1 media source for those developing the next generation mobility solutions.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Desktop Engineering

Design, simulation, test, prototyping and high performance computing.

more free magazines
 
AISI 1010
ConditionsSpecific Heat (J/kg-K)
T (°C)Treatment
50-100    450 
150-200    500 
200-250    520 
250-300    535 
300-350    565 
350-400    590 
450-500    650 
550-600    730 
650-700    825 