Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Resources
Bibliography
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

more free publications
 
AISI 1012
Category Steel
Class Carbon steel
Type Standard
Designations  United States: ASTM A29 , ASTM A510 , ASTM A519 , ASTM A545 , ASTM A549 , ASTM A575 , ASTM A576 , MIL SPEC MIL-S-11310 (CS1012) , SAE J403 , SAE J412 , SAE J414 , UNS G10120

Composition
ElementWeight %
C  0.10-0.15 
Mn  0.30-0.60 
P  0.04 (max) 
S  0.05 (max) 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  
Tensile Strength (Mpa) 370  25  cold drawn (round bar (19-32 mm)) more
Yield Strength (Mpa) 310 
Elongation (%) 19 
Reduction in Area (%) 20 
Hardness (HB) 105  25  cold drawn (round bar (19-32 mm)) more
Glossary
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.