Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Further Details
Resources
Bibliography
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free publications
 
AISI 1020
Conditions Tensile Properties 
T (°C)Treatment
25 annealed at 870°C   Tensile Strength (MPa) 394.7 
Yield Strength (MPa) 294.8 
Elongation (%) 36.5 
Reduction in Area (%) 66.0 
25 normalized at 870°C   Tensile Strength (MPa) 441.3 
Yield Strength (MPa) 346.5 
Elongation (%) 35.8 
Reduction in Area (%) 67.9 
25 rolled   Tensile Strength (MPa) 448.2 
Yield Strength (MPa) 330.9 
Elongation (%) 36.0 
Reduction in Area (%) 59.0 
Glossary
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.