Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Further Details
Resources
Bibliography
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

more free publications
 
AISI 1022
ConditionsThermal Expansion Coeff. (10-6/ºC)
T (°C)Treatment
0-100   12.2 
0-200   12.7 
0-300   13.1 
0-400   13.5 
0-500   13.9 
0-600   14.4 
0-700   14.9 
20-800   12.6 
20-1000   13.4 
Glossary
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?