Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Further Details
Resources
Bibliography
Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

more free publications
 
AISI 1023
ConditionsThermal Expansion Coeff. (10-6/ºC)
T (°C)Treatment
20-100   12.1 
20-200   12.8 
20-300   13.3 
20-400   13.9 
20-500   14.4 
20-600   14.8 
Glossary
Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.