Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Further Details
Resources
Bibliography
STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

more free publications
 
AISI 1023
ConditionsElectrical Resistivity (10-9W-m)
T (°C)Treatment
20   169 
100   219 
200   292 
400   487 
600   758 
700   925 
800   1094 
900   1136 
1000   1167 
1100   1207 
1200   1219 
1300   1239 
Glossary
STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.