Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Further Details
Resources
Bibliography
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

more free publications
 
AISI 1023
ConditionsSpecific Heat (J/kg-K)
T (°C)Treatment
50-100    486 
150-200    519 
200-250    523 
250-300    557 
300-350    574 
350-400    599 
450-500    662 
550-600    749 
650-700    846 
700-750    1432 
750-800    950 
Glossary
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.