Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Further Details
Resources
Bibliography
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

more free publications
 
AISI 1023
Conditions Tensile Properties 
T (°C)Treatment
25 cold drawn (round bar (19-32 mm))  Tensile Strength (MPa) 425 
Yield Strength (MPa) 360 
Elongation (%) 15 
Reduction in Area (%) 40 
25 hot rolled (round bar (19-32 mm))  Tensile Strength (MPa) 385 
Yield Strength (MPa) 215 
Elongation (%) 25 
Reduction in Area (%) 50 
Glossary
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!