Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Resources
Bibliography
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

more free publications
 
AISI 1026
Category Steel
Class Carbon steel
Type Standard
Designations  United States: ASTM A273 , ASTM A29 , ASTM A510 , ASTM A519 , ASTM A545 , ASTM A576 , SAE J403 , SAE J412 , SAE J414 , UNS G10260

Composition
ElementWeight %
C  0.22-0.28 
Mn  0.60-0.90 
P  0.04 (max) 
S  0.05 (max) 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.858 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  
Tensile Strength (Mpa) 490  25  cold drawn (round bar (19-32 mm)) more
Yield Strength (Mpa) 415 
Elongation (%) 15 
Reduction in Area (%) 40 
Hardness (HB) 143  25  cold drawn (round bar (19-32 mm)) more

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 12.1  20-100 more  
Thermal Conductivity (W/m-K) 51.2  100 more  
Specific Heat (J/kg-K) 486  50-100 more  

Electric Properties
Properties Conditions 
T (°C)Treatment
Electric Resistivity (10-9W-m) 169  20 more  
Glossary
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.