Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Further Details
Resources
Bibliography
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Desktop Engineering

Design, simulation, test, prototyping and high performance computing.

Autonomous Vehicle Engineering

The No. 1 media source for those developing the next generation mobility solutions.

more free magazines
 
AISI 1026
ConditionsSpecific Heat (J/kg-K)
T (°C)Treatment
50-100    486 
150-200    519 
200-250    523 
250-300    557 
300-350    574 
350-400    599 
450-500    662 
550-600    749 
650-700    846 
700-750    1432 
750-800    950 