Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Further Details
Resources
Bibliography
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Autonomous Vehicle Engineering

The No. 1 media source for those developing the next generation mobility solutions.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

more free magazines
 
AISI 1026
ConditionsThermal Conductivity (W/m-K)
T (°C)Treatment
100   51.2 
200   49 
300   46 
400   42.7 
500   39.4 
600   35.6 
700   31.8 
800   26.1 
1000   27.2 
1200   29.8 